1墙体保温材料的配比:本产品与水重量的配比是1.5:1。将材料倒入搅拌机搅拌3-5分钟可操作使用。
1 ratio of wall insulation material: the ratio of this product to the weight of water is 1.5:1. Pour the material into a blender and stir for 3-5 minutes to operate.
2在处理干净的外墙表面上可喷洒适量的清水达到墙体湿润后,将搅拌好的产品直接批抹上墙,第一遍厚度为10mm左右,大约在含水率50%时,可进行第二遍批抹,厚度为10-20mm之间。
2, on the surface of the clean exterior wall, you can spray the right amount of water to the wall to moisten it. Then stir the product directly on the wall. The thickness of the first time is about 10mm. When the moisture content is 50%, it can be batted for second times, and the thickness is 10-20mm.
3保温层厚度达到20mm要求时可一次批抹完成,厚度在30mm内可分两遍完成,凝结时间2小时左右。全部工序当天完成,八天后可粘砖、做墙体涂料饰面等。
3 insulation layer thickness to 20mm requirements can be completed once, the thickness in 30mm can be divided into two times, the setting time is about 2 hours. The whole process is completed on the day, eight days after the brick, wall paint finish.